The Textile Block System

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Textile Block System

Author(s): Edward Losch

Publication: Concrete International

Volume: 34

Issue: 3

Appears on pages(s): 45-54

Keywords: Usonian house, module, pattern, precast

DOI:

Date: 3/1/2012

Abstract:
Frank Lloyd Wright developed his textile block system for construction of middle-income housing in accordance with his Usonian concepts. Most of the houses built using the system were completed in the 1920s through the 1950s throughout the U.S. This article explores a few of the existing homes and a building currently under construction on the Florida Southern College campus, Lakeland, FL. The new building is based on Wright’s original plans, but the materials being used are more durable than those used in historical buildings.