Title: Ensuring Electrical Isolation in Elevated Rail

Author(s): Gremel

Publication: Concrete International

Volume: 34

Issue: 2

Appears on pages(s): 22-25

Keywords:

DOI:

Date: 2/1/2012

Abstract:
GFRP reinforcing bars tie rail plinths and pedestals to Miami Metrorail guideway girders