Title: ASCC Position Statement: Topping Slabs over Prestressed Members

Author(s):

Publication: Concrete International

Volume: 34

Issue: 2

Appears on pages(s): 63

Keywords:

DOI:

Date: 2/1/2012

Abstract:
Prestressed floor and roof members usually exhibit camber (upward deflection caused by eccentric prestress force).