A Review of the Durability of Glass Fiber Reinforced Concrete (GFRC), Design, and Applications

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A Review of the Durability of Glass Fiber Reinforced Concrete (GFRC), Design, and Applications

Author(s): John Jones

Publication: Symposium Paper

Volume: 280

Issue:

Appears on pages(s): 1-12

Keywords: AR glass fiber, GFRC, glass fiber reinforced concrete, acrylic polymer, pozzolans.

DOI: 10.14359/51683586

Date: 12/27/2011

Abstract:
The paper will review durability data for glass fiber reinforced concrete (GFRC), both accelerated aging and real time data. It will compare real time data with predicted data from accelerated aging tests and describe the design principles that have been established for GFRC based on this durability data. Applications over 20 years old will be reviewed.