Title: Numerical and experimental analysis of the displacements evolution of reinforced concrete beams under repeated cyclic loads

Author(s): Josafá Oliveira Filho , Gerson Moacyr Sisniegas Alva , Rejane Martins Fernandes Canha, Ana Lúcia Homce de Cresce El Debs

Publication: IBRACON

Volume: 4

Issue: 5

Appears on pages(s): 709 721

Keywords: beams, reinforced concrete, cyclic loads, damage; stiffness loss.

DOI:

Date: 11/30/2011

Abstract:
This paper discusses the structural behavior of reinforced concrete beams subjected to cyclic loadings by numerical and experimental analysis. The main objective was to quantify the increase in deflections of the beams when subjected to repeated loading cycles. Experimental tests with the application of cyclic and monotonic loading were carried out with reduced size beams. The numerical analysis utilized a simplified damage model that is part of the group denominated lumped dissipation models. This model takes into account the damage increase as a function of the increase in the number of cycles, enabling an evaluation of the stiffness loss due to repeated loads. The experimental results not only confirmed the effect of repeated loads on the stiffness loss of beams, but also demonstrated the important influence of the flexural reinforcement ratio on cyclic behavior. Comparisons between the experimental results and those obtained with the numerical model provided support for the potential of the damage model employed in the prediction of the increase of deflections caused by repeated cyclic loading.