Title: Another Look at the Drying of Lightweight Concrete

Author(s): Peter Craig and Bill Wolfe

Publication: Concrete International

Volume: 34

Issue: 1

Appears on pages(s): 53

Keywords:

DOI:

Date: 1/1/2012

Abstract:
A comparison of drying times for normalweight and lightweight floors