Title: Field Investigation of Formwork Pressures Using Self-Consolidating Concrete

Author(s): N.J. Gardner, Lloyd Keller, Robert Quattrociocchi, and George Charitou

Publication: Concrete International

Volume: 34

Issue: 1

Appears on pages(s): 41

Keywords:

DOI:

Date: 1/1/2012

Abstract:
Although progress has been made, there is no widely accepted method for predicting formwork pressures developed by self-consolidating concrete (SCC).