Interlocking Spiral Confinement for Rectangular Columns

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Interlocking Spiral Confinement for Rectangular Columns

Author(s): Samuel Yen-Liang Yin, Tzu-Liang Wu, Tony C. Liu, Shamim A. Sheikh, and Raymond Wang

Publication: Concrete International

Volume: 33

Issue: 12

Appears on pages(s): 38-45

Keywords: concrete, reinforcement, axial compression, lateral cyclic loading, design

DOI:

Date: 12/1/2011

Abstract:
Recently, an innovative interlocking multi-spiral confinement design for rectangular concrete columns was developed. This development involved testing and evaluation of a large number of full-scale reinforced concrete columns in axial compression and lateral cyclic loadings. Test results presented in this article verify that columns with interlocking multi-spiral confinement design exhibit higher compressive strength and ductility when compared to columns with conventional rectilinear hoop design. The multi-spiral confinement design was also found to be the most efficient layout in terms of automatic assembly.