Title: Concrete Q & A: Reserve Cylinders for Compressive Strength Testing

Author(s):

Publication: Concrete International

Volume: 33

Issue: 11

Appears on pages(s): 72

Keywords:

DOI:

Date: 11/1/2011

Abstract:
Is there a requirement for a minimum number of reserve cylinders? When we use 6 x 12 in. (150 x 300 mm) test cylinders (6 x 12s), we typically specify only one reserve cylinder, so is it acceptable to use only one reserve cylinder for 4 x 8 in.(100 x 200 mm) test cylinders (4 x 8s)?