Title: Concrete Technology - Volume 1 - Materials, Properties and Mix Design (SPANISH)

Author(s): Diego Sanchez de Guzman

Publication: FIHP

Volume:

Issue: 3

Appears on pages(s): 214 pgs

Keywords: Portland Cement, mortar, aggregate, additives, pozzolans, flexural test, pressure test

DOI:

Date: 4/1/2010

Abstract:
This book seeks to delve into such topics as the nature of the material, properties and characteristics of the components of concrete, illustrating the concrete as a homogeneous mixture, finalizing the design of mixtures according to the latest technologies. The content of this publication gathers the essential knowledge of the concrete technology, making basic study text for anyone interested in construction activity.