Title: Architectural Concrete (SPANISH)

Author(s): Concrete Institute

Publication: FIHP

Volume:

Issue: 1

Appears on pages(s): 115 pgs

Keywords: Finish, concrete, concrete technology, pathology, formwork, texture

DOI:

Date: 1/1/2006

Abstract:
For many years concrete has been considered one of the principal building materials. Previously, its appearance was rarely considered and only structural function was taken into account; but today, as a result of new global design trends, the professional builders are looking for new materials and perfect finish for their creations. This book is the result of information gathering, which is framed within the objective to know the management of Architectural Concrete a bit more thoroughly, looking to it to be a useful tool for the designer, builder, and everyone who is interested in revealing concrete in all their architectural creations.


Iberoamerican Federation of Ready Mixed Concrete, International Partner Access

View Resource »