Cement-Based Piezoelectric Ceramic Composite and Its Sensor Applications in Civil Engineering

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Cement-Based Piezoelectric Ceramic Composite and Its Sensor Applications in Civil Engineering

Author(s): Biqin Dong, Feng Xing, and Zongjin Li

Publication: Materials Journal

Volume: 108

Issue: 5

Appears on pages(s): 543-549

Keywords: Cement; composite; mechanic-electrical response; piezoelectric; sensor.

DOI: 10.14359/51683264

Date: 9/1/2011

Abstract:
In this study, a new kind of mechanical sensor for application in civil engineering is achieved by introducing piezoelectric ceramic into cement material, which can be used to monitor real-time structural health and provide instantaneous information on a condition of a specified structure. It is especially ideal for situ-dynamic measurement for a concrete structure, as it combines the high piezoelectric activity of piezoelectric ceramic and high mechanical properties of cement-based material. From the experimental results, a linear mechanic-electrical relationship is obtained. It is believed that cement-based piezoelectric ceramic composites hold a great application potential in civil engineering.