355.3R-11: Guide for Design of Anchorage to Concrete: Examples Using ACI 318 Appendix D

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 355.3R-11: Guide for Design of Anchorage to Concrete: Examples Using ACI 318 Appendix D

Author(s): ACI Committee 355

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 124

Keywords: anchorage; combined tension and shear; design examples; eccentric shear; embedded bolts; headed-stud anchors; post-installed anchors; shear; tension.

DOI:

Date: 3/1/2011

Abstract:
This guide presents worked examples using the design provisions in ACI318 Appendix D. Not all conditions are covered in these examples. The essentials of direct tension, direct shear, combined tension and shear, and the common situation of eccentric shear, as in a bracket or corbel, are presented.