Use of Carbon Fiber-Reinforced Polymer Anchors to Repair and Strengthen Lap Splices of Reinforced Concrete Columns

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Use of Carbon Fiber-Reinforced Polymer Anchors to Repair and Strengthen Lap Splices of Reinforced Concrete Columns

Author(s): InSung Kim, James O. Jirsa, and Oguzhan Bayrak

Publication: Structural Journal

Volume: 108

Issue: 5

Appears on pages(s): 630-640

Keywords: anchor; column; fiber-reinforced polymer (FRP); jacket; lap splice; rehabilitation; repair; strengthening

DOI: 10.14359/51683220

Date: 9/1/2011

Abstract:
The use of carbon fiber-reinforced polymer (CFRP) materials to repair and strengthen inadequate lap splices in square and rectangular reinforced concrete (RC) columns was experimentally investigated. Six large-scale columns (three square and three rectangular columns) were tested to examine the effectiveness of the rehabilitation methods for improving lap splice behavior. The test results show that a combination of CFRP jackets and CFRP anchors effectively confined short lap splices in column longitudinal reinforcement that do not comply with current lap splice provisions to transfer tensile loads. The tensile capacity of the longitudinal bars was developed and the deformation capacity of the repaired and strengthened columns was considerably improved.


ALSO AVAILABLE IN:

Electronic Structural Journal