The Silent Evolution: An Underwater Art Installation in Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Silent Evolution: An Underwater Art Installation in Concrete

Author(s):

Publication: Concrete International

Volume: 33

Issue: 8

Appears on pages(s): 34-35

Keywords: casting, marine concrete, microsilica, fiberglass reinforcing

DOI:

Date: 8/1/2011

Abstract:
Fusing public art with environmental conservation, The Silent Evolution is located in the waters of the Mexican Caribbean. More than 400 life-sized concrete sculptures of people form a complex reef structure for marine life to colonize and inhabit. Casts for the sculptures were taken from a broad cross section of society. The sculptures were built with a pH-neutral concrete—a mixture of marine-grade cement, sand, and microsilica—reinforced with inert fiberglass reinforcing bars.