Damage identification in the building's shear walls by a non-destructive method

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Damage identification in the building's shear walls by a non-destructive method

Author(s): K. Drumev, E. Milchev and A. Baltov

Publication: KILW

Volume: 50

Issue: 1

Appears on pages(s): 121-132

Keywords: non destructive testing, shear walls

DOI:

Date: 1/1/2004

Abstract:
This paper present a method for identification of the decreasing the project stiffness of building's shear walls caused by previous earthquakes, blasts, poor workmanship, careless exploitation or arbitrary reconstructions. The method is non-destructive and is based on the comparison between the dynamic parameters of the real building measured in situ with its unknown damages and the same parameters computed from the FE model of the project building. 