Self-Leveling Slab Formwork Tables Boost Efficiency

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Self-Leveling Slab Formwork Tables Boost Efficiency

Author(s):

Publication: Concrete International

Volume: 33

Issue: 6

Appears on pages(s): 23-25

Keywords: formwork, shoring, slabs, floor construction

DOI:

Date: 6/1/2011

Abstract:
To meet an accelerated construction schedule for a medical center, an innovative formwork system was used. The system comprises slab tables, supported at the column-slab interface, that automatically compensate for deflections occurring during concrete placement. After the floor concrete has reached sufficient strength to carry self-weight and construction loads, the tables are lowered and manually rolled to outrigger platforms outside the building, allowing simple and fast cycling.