Evaluating Fly Ash Blended Cements Using Rapid Chloride Permeability

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Evaluating Fly Ash Blended Cements Using Rapid Chloride Permeability

Author(s):

Publication: CIA

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 2/13/2011

Abstract:
In this study correlation between the RCPT (AASHTO-T277) and long-term ponding test was evaluated using fly ash binary blend and its ternary blends with addition of silica fume. The fly ash was used in the increasing percentage of 25, 50, and 70% of total cementitious materials, while silica fume was used at 10%. Concrete specimens were evaluated using effective w/b ratio of 0.38. Mixes were cured for a period of seven days only which relates to the general curing practice in the construction industry. The results of RCPT are supported with statistical analysis, corrosion results, pore size distribution, and microstructure evidence