The Role Of Precast Concrete As A Catalyst For Innovation

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Role Of Precast Concrete As A Catalyst For Innovation

Author(s):

Publication: CIA

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 2/13/2011

Abstract:
The precast concrete industry is often forced to be innovative to survive. Customers and designers constantly demand new solutions to old problems in both the civil engineering and building markets. The key drivers forcing change on often reluctant parties in the construction industry are listed and some examples of successful projects that have utilised innovative precast concrete alternatives to meet those needs are described.