Steel Fibres And Mesh - How They Compare For Design

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Steel Fibres And Mesh - How They Compare For Design

Author(s):

Publication: CIA

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 2/13/2011

Abstract:
Most engineers and builders accept that steel fibres provide some level of reinforcement for concrete and that the possibility exists to substitute fibre reinforcement for mesh. The problem that often arises, however, is how to simply and quickly determine the fibre dosage required to provide the same load carrying capacity as a mesh reinforced section and how a fibre reinforced element will subsequently perform in comparison. This paper addresses what are fundamental questions for designers and users of fibre reinforcement based on a design guideline.