Long Term Strength Development In Microwave Cured Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Long Term Strength Development In Microwave Cured Concrete

Author(s):

Publication: CIA

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 2/13/2011

Abstract:
The implementation of new curing technologies requires sufficient confidence on the long-term performance of the material being cured. In recent years, CSIRO has developed new rapid curing processes for precast concrete based on the use of industrial microwave heating technologies. Extensive R&D has been carried out at both bench-top and pilot scale to control bulk heating of slab type elements. Compressive strengths sufficient for formwork removal and lifting can be obtained in less than 4 hours whilst strengths sufficient for pre-stressing are achieved in less than 6 hours. These significant gains in early age strength are not accompanied by any apparent loss in medium to long-term strength development. In this Paper, medium to long-term strength development of concretes subjected to standard, conventional heat and microwave curing are discussed.