Ductility Of Reinforced Concrete Flexural Members With 500mpa Grade Steel

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Ductility Of Reinforced Concrete Flexural Members With 500mpa Grade Steel

Author(s):

Publication: CIA

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 2/13/2011

Abstract:
This paper provides a summary of the PhD research undertaken by the author to investigate the ductility and non- linear overload behaviour of reinforced concrete members constructed with 500MPa grade reinforcing steel.