The Leakage Stop of Concrete Settlement Joints in a Subway Station Using Rubber Belts

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Leakage Stop of Concrete Settlement Joints in a Subway Station Using Rubber Belts

Author(s):

Publication: CIA

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 2/13/2011

Abstract:
During the construction of Shanghai 1# metro, leakage problems were occurred in almost all the concrete joints between the main structure and passage and side tunnels due to the settlement difference and incorrect installation of rubber belt. Ordinary Slurry injection and installation of belt usually could not manage leakage problems completely. A comprehensive technology including the installation of internal changeable rubber belt, polymer injection and fillers are studied for leak-proof management, Demonstration projects indicate that leakage problems due to settlement difference between structures could be effectively prevented with this technology.