Long-Term Drying Shrinkage Measurements of Concretes made with Slag-blended Cements

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Long-Term Drying Shrinkage Measurements of Concretes made with Slag-blended Cements

Author(s):

Publication: CIA

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 2/14/2011

Abstract:
This paper presents an extensive study conducted to distinguish the factors that affect the long-term drying shrinkages of concrete containing blended cements (Type GB). Altogether 28 concrete mixes were tested up to 182 days for drying shrinkage and compressive strengths. The mixes were based on a typical Grade 32 concrete with 80 mm slump. The mixes included two types of cements (Type GP and SL) and four types of supplementary cementitious materials, namely, three types of slag and one type of fly ash. Type GB ratios of 35/65, 50/50 and 65/35 were tested. In addition to the standard tests, a modified shrinkage test was also carried out to measure the shrinkages between 0, 1, 3 and 7 days. Results show that very large strains occur between 0 and 1 day in all the concretes. Concretes containing slag exhibited expansion strains between 0 and 7 days. No appreciable expansions were observed in concretes made with Type GP cement only or with GP/fly ash blends. Based on the results, the paper questions the appropriateness of specifying standard shrinkage tests for concretes containing slag-blended cements.