Predicting Deterioration of Concrete Exposed to Biogenic Sulphuric Acid Corrosion

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Predicting Deterioration of Concrete Exposed to Biogenic Sulphuric Acid Corrosion

Author(s):

Publication: CIA

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 2/14/2011

Abstract:
A research project conducted at RMIT University aimed to investigate the deterioration of concrete septic tanks located in rural Victoria. Deterioration of the tanks could be a result of internal acid attack and external sulphate attack. A comprehensive set of laboratory experiments was established to measure the accelerated deterioration of concrete under exposure to sulphate and acid. The mass changes in concrete specimens have been recorded for a period of one year when exposed to sulphate solutions and sulphuric acid solutions. The specimens were manufactured using the same mix design and ingredients used in septic tank production in the country Victoria prior to 1990. Based on the changes of mass recorded over the one year period, a statistical model has been developed to predict the mass loss/gain of concrete with time as a function of the cement content, and acid concentration observed in sewerage.