The Evolution of Architectural Precast Concrete Facades in Australia over the last 50 years

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Evolution of Architectural Precast Concrete Facades in Australia over the last 50 years

Author(s):

Publication: CIA

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 2/28/2011

Abstract:
Precast facades in Australia have evolved over the past 50 years from simple small panels with basic finishes to the sometimes complex panels with high quality finishes of today. There have been some problems and lessons leant over that time. As we move forward into the new millennium, ingenuity and creativity along with the appropriate skills, design and sustainability will be the key issues for precast concrete facades for the future.