Strength and Hydration Heat of Concrete using Fly Ash as a Partial Replacement of Cement

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Strength and Hydration Heat of Concrete using Fly Ash as a Partial Replacement of Cement

Author(s):

Publication: CIA

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 2/28/2011

Abstract:
The benefits of using fly ash as a partial replacement for cement in concrete are well documented. This paper presents the strength development and hydration heat properties of concrete using Class F fly ash sourced from Western Australia. Compressive strengths at different ages were determined and semi-adiabatic temperature rise during the initial stage of hydration was measured by thermocouples. The 28-day compressive strengths of two control concrete mixtures were 62 and 68 MPa. It was found from the experimental results that the average 28-day compressive strengths of concretes with 30% and 40% cement replacements by fly ash were 84% and 63% of the strengths of the respective control mixtures. However, the 90-day strength of concrete with 30% cement replacement was equal to the strength of the control concrete. A 20% reduction in the maximum temperature was observed in the concrete with 40% cement replacement by the fly ash. It is found from the test data that the percentage reduction in the maximum temperature of fly ash concrete can be estimated as one-half of the percentage replacement of cement by fly ash.