Models for Inelastic Analysis of FRP Reinforced Concrete Members

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Models for Inelastic Analysis of FRP Reinforced Concrete Members

Author(s):

Publication: CIA

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 2/28/2011

Abstract:
Inelastic behaviour of FRP reinforced concrete beams and columns is usually modelled using one of two different methods. The first method is based on an associative plasticity model for the concrete, in which gradual compressive crushing or tensile cracking on the cross-section, as well as along the member, is considered. The FRP reinforcement exhibits linear elastic response up until brittle fracture at a relatively high fracture strain. The second method is based on an experimentally developed moment displacement relationship for the member. For this model the inelastic behaviour is assumed to be lumped at springs connected to the ends of the member. Computer programs are developed which incorporate these models and results based on both models are compared for the cases of a cantilever column and a structural frame.