Title: Restoration of the Newcastle Civic Theatre

Author(s):

Publication: CIA

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 2/28/2011

Abstract:
The purpose of this paper is to provide a brief account of how the external façade of the Newcastle Civic Theatre was upgraded. The façade showed signs of structural and corrosion stress. Tried and proven concrete, electrochemical and epoxy repair techniques together with application of an engineered protective coating was able to extend the building’s service life.