Z 03 - Grouting of Prestressing Ducts

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Z 03 - Grouting of Prestressing Ducts

Author(s):

Publication: CIA

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 11/19/2010

Abstract:
Experience with grouted post-tensioning tendons over half a century has proven that a cementitious grout can provide an excellent protection to the prestressing steel. Experience has also shown that the quality of the grouting is of prime importance for the durability of post-tensioning tendons for any kind of application (bonded internal tendons, external tendons, slab tendons, stressbars, ground anchors, and stay cables). Incomplete or no grouting has been the origin of a range of problems from corrosion to delayed failures of tendons or parts of tendons. Better quality of grouting materials and of on site grouting activities are a small marginal cost to the owner compared to the consequences of poor or improper grouting.