Z 05 - Shotcreting in Australia

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Z 05 - Shotcreting in Australia

Author(s):

Publication: CIA

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 11/19/2010

Abstract:
This document has been written as a guide to the use of shotcrete in Australia. It is based on established practice within the Australian context and is targeted toward designers, specifiers, owners, suppliers, contractors and other end users of shotcrete. From limited beginnings in the 1960s, shotcrete has emerged as the first choice for ground support in the general construction and mining industries and is increasingly being used in other applications. Shotcrete is an evolving technology and users of this guide must appreciate that the contents represent the state of knowledge and practice at the date of publication and may be subject to change.