Early Age Strength Properties of High Performance Concrete Under Accelerated Curing

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Early Age Strength Properties of High Performance Concrete Under Accelerated Curing

Author(s):

Publication: CIA

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 2/13/2011

Abstract:
Cementitious systems used in precast elements that undergo an accelerated curing regime usually have tight specifications with regards to early age compressive strength requirements. Super T beams cast for the Melbourne Eastlink Freeway called for 40MPa transfer strength at 14 hours and adherence to VicRoads Section 610 (1) on structural concrete cured under radiant heating. Concrete test cylinders cast for the purpose of determining transfer strengths were required to be placed in heating boxes that were connected to the hot water heating system. They were found not to be good representations of insitu concrete compressive strengths. Early age strengths of the beam elements were successfully predicted using the maturity method and the temperature matched curing system. Trials were also conducted using different ways of administering high range water reducers (superplasticisers) to improve concrete performance.