Sulfate-resisting concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Sulfate-resisting concrete

Author(s): Cement Concrete & Aggregates Australia

Publication: CCAA

Volume:

Issue:

Appears on pages(s): 8 pages

Keywords: sulfate resisting cement, permeability, sulfate, expansion, strength retention

DOI:

Date: 9/1/2007

Abstract:
This Technical Note reports the outcome of a research project conducted by CCAA. In this project the performance of ten concrete mixes proportioned using five sulfate resisting cements complying with AS 3972 was evaluated. The results were examined in relation to long-term concrete exposure data. It also reviews current specifications for sulfate resisting concrete in the context of the research findings.


Cement Concrete & Aggregates Australia, International Partner Access

View Resource »