Title: Seismic retrofitting of RC Shear wall with external bonded CFRP

Author(s): S. Qazi, E. Ferrier, L. Michel, P. Hamelin

Publication: Symposium Paper

Volume: 275

Issue:

Appears on pages(s): 1-20

Keywords: Retrofitting, seismic, RC wall, CFRP

DOI: 10.14359/51682463

Date: 3/1/2011

Abstract:
Shear walls as an integral part of structures have revealed to be of prime concern following earthquake surveys over the past few years. It was observed that shear wall structures sustained less damage in comparison to structures that did not possess shear wall. Researchers on the basis of their post earthquake surveys concluded that shear wall buildings sustained damage as a result of design and construction work flaws. In this article test data of CFRP strengthened short RC walls is analyzed. Three RC shear walls, designed to fail in shear, were subjected to static and cyclic load tests in which the loading amplitude was gradually increased till specimen failure occurred. Two out of three walls were strengthened externally with the help of CFRP material and mesh anchors at the wall foundation joint. The experimental results analysis consists in cracking pattern, stiffness, ultimate load capacity, ductility and energy dissipation.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer