Shear Strengthening RC T-beams Using CFRP Laminates and Anchors

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shear Strengthening RC T-beams Using CFRP Laminates and Anchors

Author(s): Yungon Kim, Kevin T. Quinn, Christopher N. Satrom, Wassim M. Ghannoum, and James O. Jirsa

Publication: Symposium Paper

Volume: 275

Issue:

Appears on pages(s): 1-18

Keywords: CFRP, CFRP anchor, reinforced concrete, T-beam , Shear strengthening,

DOI: 10.14359/51682446

Date: 3/1/2011

Abstract:
Several tests were conducted to evaluate the shear performance of beams strengthened externally with carbon fiber reinforced polymer (CFRP) laminates and CFRP anchors. Results are presented for five tests conducted on 24-in.(610-mm) deep reinforced concrete T-beams constructed and tested at Phil M. Ferguson Structural Engineering Laboratory at the University of Texas at Austin. Monotonically increasing load was applied to the reinforced concrete members at a shear span-to-depth ratio of three (a/d = 3) until failure. Overall, a 40-45% increase in shear strength was observed when anchored CFRP laminates were installed on the RC members. In all cases, CFRP anchors prevented a premature de-bonding failure in the CFRP laminates, thus increasing the useable capacity of the CFRP laminates. Theoretical calculations predicting the shear strength of the retrofitted concrete members were carried out and compared with the measured strengths of the members.