Analysis of CFRP Strap-Strengthened Reinforced Concrete Beams Using the Modified Compression Field Theory (MCFT)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Analysis of CFRP Strap-Strengthened Reinforced Concrete Beams Using the Modified Compression Field Theory (MCFT)

Author(s): Hiran D. Yapa and Janet M. Lees

Publication: Symposium Paper

Volume: 275

Issue:

Appears on pages(s): 1-20

Keywords: Concrete beams, Fibre reinforced polymer, MCFT, Shear

DOI: 10.14359/51682441

Date: 3/1/2011

Abstract:
External, prestressed carbon fiber reinforced polymer (CFRP) straps can be used to enhance the shear strength of existing reinforced concrete beams. In order to effectively design a strengthening system, a rational predictive theory is required. The current work investigates the ability of the modified compression field theory (MCFT) to predict the behavior of rectangular strap strengthened beams where the discrete CFRP strap forces are approximated as a uniform vertical stress. An unstrengthened control beam and two strengthened beams were tested to verify the predictions. The experimental results suggest that the MCFT could predict the general response of a strengthened beam with a uniform strap spacing < 0.9d. However, whereas the strengthened beams failed in shear, the MCFT predicted flexural failures. It is proposed that a different compression softening model or the inclusion of a crack width limit is required to reflect the onset of shear failures in the strengthened beams.