Volumetric Response of FRP-Confined Full-Scale RC Columns

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Volumetric Response of FRP-Confined Full-Scale RC Columns

Author(s): Antonio De Luca, Fabio Nardone, Fabio Matta, Gian Piero Lignola, Andrea Prota, and Antonio Nanni

Publication: Symposium Paper

Volume: 275

Issue:

Appears on pages(s): 1-22

Keywords: Confinement, Deformability, FRP laminates, Full-scale RC columns, Strengthening, Volumetric strain.

DOI: 10.14359/51682420

Date: 3/1/2011

Abstract:
The external confinement of reinforced concrete (RC) columns by means of externally bonded fiber reinforced polymer (FRP) laminates is a well established technique for strengthening and retrofitting purposes. This paper presents a pilot research that includes laboratory testing of full-scale square and rectangular (with side-aspect ratio smaller than 1.5) RC columns externally confined with glass and basalt-glass FRP laminates and subjected to pure axial load. Specimens that are representative of full-scale building columns were designed according to a dated ACI 318 code (i.e., prior to 1970) for gravity loads only. The study was conducted to investigate how the external confinement affects peak axial strength and deformation of a prismatic RC column. The results showed that the FRP confinement increases concrete axial strength, but it is more effective in enhancing concrete strain capacity.