222.3R-11: Guide to Design and Construction Practices to Mitigate Corrosion of Reinforcement in Concrete Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 222.3R-11: Guide to Design and Construction Practices to Mitigate Corrosion of Reinforcement in Concrete Structures

Author(s): ACI Committee 222

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 28

Keywords: admixtures; aggregates; aluminum; cathodic protection; cement; chlorides; consolidation; corrosion; curing; epoxy coating; high-range water-reducing admixtures; mixing; mixture proportioning; permeability; reinforcing steel.

DOI:

Date: 4/1/2011

Abstract:
Corrosion of metals in concrete is a significant problem throughout the world. In many instances, corrosion can be avoided if proper attention is given to detailing, concrete materials and mixture proportions, and construction practices. This guide contains information on aspects of each of these. In addition, the guide contains recommendations for protecting in-service structures exposed to corrosive conditions. The guide is intended for designers, materials suppliers, contractors, and all others engaged in concrete construction.




  