An Electric Freeway to the Future

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: An Electric Freeway to the Future

Author(s): Bruce W. Ramme and Steven H. Miller

Publication: Concrete International

Volume: 33

Issue: 5

Appears on pages(s): 45-48

Keywords: fly ash, carbon, grounding, sheilding

DOI:

Date: 5/1/2011

Abstract:
Electrically conductive high-carbon concrete (HCC) is being developed and could potentially be used for many new technological advances. Carbon from high-carbon fly ash and spent carbon sorbent—both byproducts of coal combustion in modern power plants—make HCC a conductor. Initial HCC applications have included low-cost grounding for lightning-vulnerable structures, but a much wider range of use is envisioned, including electrical shielding, self-deicing bridges, induction-charging of electric vehicles, and pavements that function as storage batteries. This article explores some of these possibilities.