Title: SP-278: Frontiers in the Use of Polymers in Concrete

Author(s): Editor: Mahmoud Reda Taha / Sponsored by Committee 548

Publication: Symposium Paper

Volume: 278

Issue:

Appears on pages(s): 163

Keywords:

DOI: 10.14359/51682357

Date: 3/1/2011

Abstract:
This CD-ROM contains nine papers sponsored by ACI Committee 548. The extended use of polymers in concrete has grown significantly in the last two decades. This is demonstrated from the common use of epoxy to repair cracks, to the use of polymer concrete overlays to protect bridge decks. The papers provide insight into the current state of research and development for the use of polymers in concrete and new trends that will shape the frontiers of the polymer concrete industry in the near future. Note: The individual papers are also available. Please click on the following link to view the papers available, or call 248.848.3800 to order. SP-278


Product unavailable, please call +1.248.848.3800