Title: SP-276: Durability Enhancements in Concrete with Fiber Reinforcement

Author(s): Editors: Corina-Maria Aldea and Nur Yazdani / Sponsored by: ACI Committee 544

Publication: Symposium Paper

Volume: 276

Issue:

Appears on pages(s): 120

Keywords:

DOI: 10.14359/51682325

Date: 3/1/2011

Abstract:
This CD-ROM contains six papers that were presented at sessions sponsored by ACI Committee 544 at the Spring 2008 ACI Convention in Los Angeles, CA, and the Spring 2009 ACI Convention in San Antonio, TX. The papers provide insight into the state of the art of the topic in academia, the industry, and real-life applications and cover some of the benefits of using fibers to enhance long-term performance of concrete with and without conventional reinforcement. Note: The individual papers are also available. Please click on the following link to view the papers available, or call 248.848.3800 to order. SP-276