Another Look at the Relationship between Strength and Composition of Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Another Look at the Relationship between Strength and Composition of Concrete

Author(s): Sandor Popovics

Publication: Materials Journal

Volume: 108

Issue: 2

Appears on pages(s): 115-119

Keywords: cement content; composite; model; modulus; water-cement ratio

DOI: 10.14359/51682304

Date: 3/1/2011

Abstract:
This paper contributes to the relationship between the concrete strength and its composition by offering novel, multi-variable formulas for the concrete strength-versus-composition relationship.


ALSO AVAILABLE IN:

Electronic Materials Journal