350.1-10: Specification for Tightness Testing of Environmental Engineering Concrete Containment Structures and Commentary

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 350.1-10: Specification for Tightness Testing of Environmental Engineering Concrete Containment Structures and Commentary

Author(s): ACI Committee 350

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 15

Keywords: containment structures; hydrostatic; leakage; pneumatic; reservoirs; tests; tightness; tightness criteria.

DOI:

Date: 1/1/2011

Abstract:
These test methods give procedures and criteria for tightness testing of environmental engineering concrete structures. They are applicable to liquid and gas containment structures constructed with concrete or a combination of concrete and other materials. This document includes hydrostatic, surcharged hydrostatic, and pneumatic tests. These test methods may involve hazardous materials, operations, and equipment. This document does not purport to address all of the safety problems associated with its use. It is the responsibility of the user of this document to establish appropriate safety and health practices and determine the applicability of regulatory limitations before use.