Title: Concrete Q & A: Curing Concrete with Saturated Burlap or Curing Compound

Author(s): JoAnn Browning and David Darwin

Publication: Concrete International

Volume: 33

Issue: 3

Appears on pages(s): 88

Keywords:

DOI:

Date: 3/1/2011

Abstract:
Many of our projects are in Saudi Arabia. Our standard specification calls for 7 days of wet curing using saturated burlap, but contractors have asked us to allow the use of curing compounds for flatwork. What are the tradeoffs?