Research on the Production Technology of Recycled Aggregate

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Research on the Production Technology of Recycled Aggregate

Author(s): Rongjun Gu, etc.

Publication: China Concrete and Cement Products

Volume:

Issue: No.1 2010(Total 171)

Appears on pages(s): 16-18

Keywords: Waste concrete, Recycled aggregate, Production technology, Mobile production, Classifiable specialization

DOI:

Date: 2/20/2010

Abstract:
Based on comprehensive analysis of the production technology of recycled aggregate at home and abroad, the classified recovery of waste concrete is proposed for the current problems in recycled aggregate production. And the models of recycled aggregate production of mobile and classifiable specialization are maded for different types of waste concrete, which have their respective production process.