Experimental Research on the Toughness of RPCC with SHPB Technology

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Research on the Toughness of RPCC with SHPB Technology

Author(s): Rui Wang, etc.

Publication: China Concrete and Cement Products

Volume:

Issue: No.2 2010(Total 172)

Appears on pages(s): 13-15

Keywords: RPCC, SHPB, Dynamic properties, Toughness

DOI:

Date: 4/20/2010

Abstract:
The Rubberized Portland Cement Concrete (RPCC) is prepared by adding proper rubber powder into cement concrete,and the rubber powder can improve the toughness and impact resistance of concrete.The performance of impact resistance of RPCC is studied by using the experimental technology of Split Hopkinson Pressure Bar (SHPB).The stress-strain curve under different strain rates and toughness index are obtained for RPCC,and the influences of rubber powder particle sizes and dosage on dynamic properties of concrete are analyzed and discussed.