Parameters Optimization of Electrochemical Chloride Extraction and Exploratory Research on its Engineering Application

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Parameters Optimization of Electrochemical Chloride Extraction and Exploratory Research on its Engineering Application

Author(s): Pin Zhu, etc.

Publication: China Concrete and Cement Products

Volume:

Issue: No.2 2010(Total 172)

Appears on pages(s): 4-8

Keywords: Electrochemical chloride extraction, Parameters optimization, Engineering application

DOI:

Date: 4/20/2010

Abstract:
On the basis of parameters optimization of electrochemical chloride extraction(ECE),exploratory research on its engineering application is carried out.The results show that chloride ion in ECE treated concrete with saturated Ca(OH)2 solution(0.001mol/L Li2B4O7) as electrolyte and 2A/m2 current density can be extracted by 80%,and there is no obviously harmful effect on its compressive strength and impermeability.
To order a copy of this publication EMail CCPA at Qinghuan Zhang


China Concrete and Cement Products, International Partner Access