Study on Concrete Damage Experiment under Sulfate Attack and Freeze-thaw Cycles

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Study on Concrete Damage Experiment under Sulfate Attack and Freeze-thaw Cycles

Author(s): Xinzheng An, etc.

Publication: China Concrete and Cement Products

Volume:

Issue: No.2 2010(Total 172)

Appears on pages(s): 1-3

Keywords: Pumping concrete,Sulfate attack, Immersion-dry cycles, Freeze-thaw cycles, Damage

DOI:

Date: 4/20/2010

Abstract:
In the process of life-cycle of concrete,sulfate attack and freeze-thaw cycles are two important factors that affect the durability of concrete structures.The damage process of pumping concrete with water to cement ratio of 0.44 under immersion-dry cycles or immersion-dry-freeze-thaw cycles in solutions of 6.0% Na2SO4 is studied.The results show that the relative dynamic modulus of elasticity Erd increases linearly and the damage variable Dm(T)=0 in the initial stage of immersion-dry cycles,but according to the immersion-dry cycles increased,the damage variable D experienced the process from 0 to slow increasing,at last rapid increasing,and the relative dynamic modulus of elasticity Erd experienced the process from increasing linearly to decreasing slowly.Compared with the immersion-dry cycles,the interactive effects of immersion-dry cycles and freeze-thaw cycles have greatly accelerated the process of concrete damage.