Title: Ground Load Calculation of Buried Rigid Pipes

Author(s): Xiaoping Que and Pingmu Li

Publication: China Concrete and Cement Products

Volume:

Issue: No.3 2010(Total 173)

Appears on pages(s): 26-31

Keywords: Buried rigid Pipes, Additional load, Accumulated load, Stress dispersion angle method, Additional stress method

DOI:

Date: 6/20/2010

Abstract:
For the role of buried rigid pipes on the ground load,the difference between additional load and accumulated load is studied,and through several calculation methods analysing and examples calculating,the clear parameters for ground load calculations are proposed,and the applicable calculation methods under different load conditions are gained.