Characteristics and Applications of Nano Micro-bead(N-MB)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Characteristics and Applications of Nano Micro-bead(N-MB)

Author(s): Naiqian Feng and Hao Li

Publication: China Concrete and Cement Products

Volume:

Issue: No.5 2010(Total 175)

Appears on pages(s): 1-3

Keywords: Nano micro-bead,High performance concrete,Ultra-high performance concrete,Application

DOI:

Date: 10/20/2010

Abstract:
Nano micro-bead(N-MB) is a superfine glass bead from the smoke discharged by coal station,whose average particle size is ≦1.0μm.The surface of N-MB is vitreous body,which shows spherical.The mixed water for concrete can be reduced and the fluidity of concrete is increased when the N-MB is partly instead of cement and added into concrete.The strength and durability of the concrete will be increased by using the N-MB for concrete.And the N-MB is one new component in concrete low carbon technology.The applica-tion of N-MB is introduced in the high performance concrete and ultra-high performance concrete.